Home > News > Content

Tungsten Carbide Chemical Properties

Jan 30, 2021

The active oxidation starts when the temperature is above 500℃ in the air, and the anti-oxidation ability is weak.


Strong acid resistance.


Chemical reaction formula: W + C = WC Note: React at 1150℃.


It does not react with chlorine below 400°C; it can react violently with fluorine at room temperature; it is oxidized to tungsten oxide when heated in the air.

Send Inquiry